dc.contributor.authorBourne, N. K.; email: neil.bourne@manchester.ac.uk
dc.contributor.authorMirihanage, W. U.
dc.contributor.authorOlbinado, M. P.
dc.contributor.authorRack, A.
dc.contributor.authorRau, C.
dc.date.accessioned2021-06-25T15:26:18Z
dc.date.available2021-06-25T15:26:18Z
dc.date.issued2020-06-25
dc.date.submitted2019-12-31
dc.identifierhttps://chesterrep.openrepository.com/bitstream/handle/10034/625043/41598_2020_Article_67086.pdf?sequence=2
dc.identifierhttps://chesterrep.openrepository.com/bitstream/handle/10034/625043/41598_2020_Article_67086_nlm.xml?sequence=3
dc.identifier.citationScientific Reports, volume 10, issue 1, page 10366
dc.identifier.urihttp://hdl.handle.net/10034/625043
dc.descriptionFrom Springer Nature via Jisc Publications Router
dc.descriptionHistory: received 2019-12-31, accepted 2020-05-28, registration 2020-06-03, pub-electronic 2020-06-25, online 2020-06-25, collection 2020-12
dc.descriptionPublication status: Published
dc.description.abstractAbstract: To travel safely behind screens that can protect us from stones and hail, we must understand the response of glass to impact. However, without a means to observe the mechanisms that fail different silicate architectures, engineering has relied on external sensors, post-impact examination and best-guess to glaze our vehicles. We have used single and multi-bunch, X-ray imaging to differentiate distinct phases of failure in two silicates. We identified distinct micromechanisms, operating in tandem and leading to failure in borosilicate glass and Z-cut quartz. A surface zone in the amorphous glass densifies before bulk fracture occurs and then fails the block, whilst in quartz, fast cracks, driven down cleavage planes, fails the bulk. Varying the rate at which ejecta escapes by using different indenter tip geometries controls the failed target’s bulk strength. This opens the way to more physically based constitutive descriptions for the glasses allowing design of safer, composite panels by controlling the impulses felt by protective screens.
dc.languageen
dc.publisherNature Publishing Group UK
dc.rightsLicence for this article: http://creativecommons.org/licenses/by/4.0/
dc.sourceeissn: 2045-2322
dc.subjectArticle
dc.subject/639/166/988
dc.subject/639/301/1023/218
dc.subject/639/766/25
dc.subject/639/766/930/12
dc.subjectarticle
dc.titleImpact failure in two silicates revealed by ultrafast, in situ, synchrotron X-ray microscopy
dc.typearticle
dc.date.updated2021-06-25T15:26:18Z
dc.date.accepted2020-05-28


Files in this item

Thumbnail
Name:
41598_2020_Article_67086.pdf
Size:
1.695Mb
Format:
PDF
Thumbnail
Name:
41598_2020_Article_67086_nlm.xml
Size:
76.54Kb
Format:
XML

This item appears in the following Collection(s)